No one sells more DSC’s than TA Instruments. From the most cost-effective DSC with industry-leading performance, to the most advanced DSC available, there is a TA Instruments DSC to meet your needs and exceed your expectations.
DSC25 | DSC250 | DSC2500 | X3 DSC | DSC 25P | ||
---|---|---|---|---|---|---|
Baseline Flatness (-50 to 300°C)[1] | ≤100 μW | ≤10 μW | ≤5 μW | ≤10 μW | - | |
Baseline Repeatability (-50 to 300°C) | <40μW | <20μW | <10μW | <15μW | - | |
Temperature Range | -180°C to 725°C | -180°C to 725°C | -180°C to 725°C | -180°C to 550°C | RT to 550°C | |
Temp Accuracy | ±0.1°C | ±0.05°C | ±0.025°C | ±0.025°C | - | |
Temp Precision | ±0.01°C | ±0.008°C | ±0.005°C | ±0.005°C | - | |
Enthalpy Precision | ±0.1% | ±0.08% | ±0.04% | ±0.08% | ||
[1] No Baseline subtractions Find out more information about DSC 25P in the next section |
The DSC 25 offers exceptional DSC performance, even against many competitive top-of-the-line instruments. With standard Modulated DSC® and the option to add an autosampler, all in a cost-effective package, getting great DSC data at a reasonable price has never been easier! The Discovery DSC 25 is the ideal instrument for industrial, quality control, and teaching laboratories.
Key Features
The DSC 250, with patented Tzero® Technology, easily outperforms competitive top-of-the-line models. Our versatile instrument is upgradeable with a 64 position autosampler and compatible with the photocalorimeter and microscope accessories. The Discovery DSC 250 is the ideal choice across a range of laboratory needs.
Key Features
The DSC 2500 is designed for researchers that require the highest level of performance and features in one package. Patented T4P Tzero® heat flow delivers the highest sensitivity and resolution, along with the ability to make heat capacity measurements in a single run.
Key Features
TA Instruments invites you to Discover the possibilities with the Discovery X3 Differential Scanning Calorimeter featuring a multi-sample cell that delivers high quality heat flow data for up to three samples simultaneously. The Discovery X3 DSC combines industry-leading performance with the tools to increase productivity on every level of material research. TA Instruments’ commitment to innovation enables scientists and engineers to reach their goals faster and make critical decisions with confidence.
Key Features
|
DSC 25P
|
---|---|
Pressure Range
|
Up to 7MPa or 1000PSI
|
Temperature Range (standard)
|
RT to 550°C
|
Temperature Range with cooling accessory
|
-130°C to 550°C
|
Purge Gas
|
N2, Air, O2, He, Ar, CO2, CO, H2
|
The DSC 25P is a dedicated Pressure DSC module that provides heat flow measurements on pressure sensitive materials. The Discovery DSC 25P is used to study thermal transitions, chemical reactions and oxidative stability/ decomposition under vacuum, standard atmospheric pressure and elevated pressures. It measures a materials’ heat flow in a variety of inert, oxidizing or reducing atmospheres. The DSC 25P has a pressure range of 1 Pa to 7 MPa (0.0001 to 1,000 psi) of which experiments can be performed under static or dynamic purge (constant volume or constant pressure). The Discovery DSC 25P can operate under atmospheric and elevated pressures from ambient to 550 °C. The optional Quench Cooling Accessory for the FACS extends the operational temperature range of the DSC 25P down to -130°C.
Key Features
Nano DSC is a high-resolution method for quantifying the thermal stability of large biomolecules and biotherapeutics. This instrument measures the heat of reaction from tertiary and secondary structure changes that occur when a biomolecule unfolds, or melts in the case of nucleic acids and lipids. The Nano DSC provides peak temperature when unfolding occurs and a total heat from the unfolding event.
The Nano DSC is a highly sensitivity differential scanning calorimeter for testing liquid samples containing a biomolecule or biotherapeutic sample. The unit is software controlled and experiments are set up, so that a sample is heated at a controlled rate over a defined temperature range. The Nano DSC can be automated to deliver samples directly from temperature-controlled 96 well plates, for unattended use. Automated cleaning eliminates sample carryover effects, and automated sample loading ensures the sample is delivered to the instrument the same way, every time.